Excerpt from  ISO 13847 (Petroleum and natural gas industries - Pipeline transportation systems - Welding of pipelines)

7
Production welding
7.1 General
The distance between girth welds, circumferential fillet welds and branch welds should not be less than the outside diameter of the pipe.

ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,

Nandesh Kumar A

Abu Dhabi, UAE

P.S. : Please don't print this e-mail unless you really need to.


--- On Wed, 26/12/12, Gane Nalla <gane2478@hotmail.sg> wrote:

From: Gane Nalla <gane2478@hotmail.sg>
Subject: RE: [MW:16334] minimum length of pipe in the subsea spool..
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Wednesday, 26 December, 2012, 8:41 AM

Hi, Chandra
Normal Industrial Practise- Min 4 x pipe thk. or 100mm whichever greater
Normally it dictated ny Client Spec. or in Engineering Dwgs.
I dont think so codes dictates that.
Hope i'm correct
Welcome more inputs as this question often raised

 
Thank and With Warmest Regards
 
Ganesan
 

 

Date: Tue, 25 Dec 2012 23:37:06 -0800
From: bocant_btm@yahoo.com
Subject: [MW:16330] minimum length of pipe in the subsea spool..
To: materials-welding@googlegroups.com

deat expert,

i want to ask about,how length minimum of the pipe if any additional joint in the subsea pipe/pipeline.
i try to search in the ASME B31.8 and other spec about pipeline, i dont find minimum length of pipe/distance between weld to weld.
can somebody advise for me,where the spec will be use?!
Thanks for your time and attention.
 
Regards,
Chandra Putra

Skype: chandra.putra12

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...