Re: [MW:16335] minimum length of pipe in the subsea spool..

500mm as per BSEN 12952

On Wed, Dec 26, 2012 at 1:07 PM, chandra putra <bocant_btm@yahoo.com> wrote:
deat expert,

i want to ask about,how length minimum of the pipe if any additional joint in the subsea pipe/pipeline.
i try to search in the ASME B31.8 and other spec about pipeline, i dont find minimum length of pipe/distance between weld to weld.
can somebody advise for me,where the spec will be use?!
Thanks for your time and attention.
 
Regards,
Chandra Putra

Skype: chandra.putra12

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...