Tuesday, December 25, 2012

Re: [MW:16325] Reg:Welding of dissimilar thickness joints of dissimilar P-No.

Dear Avinash

Simply we can qualify with 70 to 80% of weld metal thickness with
refference to thinner metal joined. i.e if u r welding 10mm to 20mm
means weld thick can be around 7-8mm.


Regards
Ambrish
Sr. Engg. - QA

On 12/24/12, Avinash Pandey <avi7589@gmail.com> wrote:
> Dear Expert
>
> Please help me out regarding a query.
>
> 1. If I will be welding 10thk # 20thk plate test coupon of P-No.1 and
> P-No.11A than how much base metal as well as weld metal will be qualify.
>
> 2.Please also give me the interpretation for QW.202.4 (Dissimiler metal
> thickness clauses) in simple english, taht will be very helpful to me
>
> Regards
> Avinash Pandey
>
> Trainee
> Welding Dept.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...