Dear Mr Ashok As far as I know We can not weld Aluminum to CS except Brazing Regards Hegde p.B.
--- On Mon, 24/12/12, Ashok Shende <shendeashok08@rediffmail.com> wrote:
From: Ashok Shende <shendeashok08@rediffmail.com> Subject: [MW:16315] Filler wire for Aluminium to CS TIG welding To: materials-welding@googlegroups.com Date: Monday, 24 December, 2012, 9:32 AM
Dear experts we are having a project of aluminium heat exchangers with tube side MOC as aluminium SB 209. Here I want to make confirm the suitable filler wires for TIG welding of Aluminium to SA 516 GR 60/70. Thanks in advance. Catch India as it happens with the Rediff News App. To download it for FREE, click here -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/ http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments