Dear Lassaad

first you should inspected it visually. Specially you pay attention to
important area such as sumps, three-plate laps, arc strikes, temporary
attachment removal areas.
Then All of bottom plate overlaps shall be tested by VBT(vacuum box test).

Also you can see 7.3.3 from API 650(2007).


Best Regards,
Farhang





-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Lassaad
Sent: Sunday, December 30, 2012 7:19 PM
To: materials-welding@googlegroups.com
Subject: [MW:16377] TANK BOTTOM PLATES OVERLAP

Dear Experts,
Is there any NDT method to check the overlap of bottom plates of an API650
built and used Oil steel tank.?
Many thanks
BR

Sent from my iPad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=
anet_ug_hm

The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...