[MW:16350] Re: Grinding or filling is allowed on Final pass (on capping) for WPQT ? Urgent plse..

dear,
Cleaning is allowed.after capping,filling&repairing on weld are not
allowed.

Regards,
Mohd.

On Dec 27, 12:07 pm, Sathish Kumar <sathishbem...@gmail.com> wrote:
> Dear Experts,
> Please advice.
> whether Grinding or filling is allowed on Final pass (on capping) for
> Welder performance qualification test (WPQT) for Plate or Pipe. Since
> qualification is done based on ASME Sec 9, so i need reference only as per
> ASME Sec 9.
> Also already i referred ASME Sec 9 - QW194, which only mentions the
> Complete joint penetration for visual examination for WPQT. But it is not
> more specific in case of Grinding or filling and also some other
> (acceptable limits ? )parameters like Reinforcement, undercut, underfill
> etc..
> I need only Asme Sec 9 reference, because as per the project contract only
> Asme Sec 9 is applicable for our project in case of WPQT.
> please advice guys..
> Thanks in advance..
>
> Regards
> sathish. K
> Welding inspector.
> Jubail, Saudi arabia.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...