Wednesday, October 3, 2012

Re: [MW:15460] Number of welder to be used/allowed as per API1104 and ASMEIX

Mr. Mohammed,

It is a question of easiness of operation and speed of welding (no. of joints to be done per unit time)that decides the no. of welders to be used in the cross country piping.

Up to say 12" one welder can be used or even two if the speed of line welding to be increased.

Beyond 14" and up to 42" or nearest two welders are used,If the trench permits i.e.,
if there is enough place for welders, even 4 could be used for 42" size.

4 welders are idle for size 48" and above as it will be difficult to get a reach with 2 welders.

The pipe is divided in 4 segments and ladders are used to get a reach for upper segments on either side, while 2 welders complete both bottom segments.

Sridhar.


From: Vajjiravelu Ravi <vajjiraveluravi3@gmail.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, 3 October 2012 2:29 PM
Subject: Re: [MW:15458] Number of welder to be used/allowed as per API1104 and ASMEIX

In API 1104 IT IS ESSENTIAL VARIABLE TO BE FOLLOWED IN WELDER SELECTION UNABLE TO GIVE THE LOCATION/ CODE HEADING 

PL CROSS CHECK IN API 1104 - FOR OTHER CODE I AM NOT SURE 

On Wed, Oct 3, 2012 at 11:43 AM, mohd <mohd52100@gmail.com> wrote:
Dear all,


Is there anywhere mentioned (Code :API1104/ASME-IX) number of welders to be used for Diameter range?

I want expert opinion and Generally using/allowing number of welders for various diameter range (6" to 72").


regards,
mohammed.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
Vajjiravelu Ravi
Welding,Painting,NDT & ISO 9001/2008
 
take all steps to save our health  wealth & environment.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...