Hi,
Single welder groove weld with backing,double welded welds,partial penetration groove welds are considered as Weld With Backing.
WPS qualified with Backing can be qualified for Weld with backing and all fillet welds.
In your case, you can use this WPS for all Fillet welds and you need to revise your WPS qualification as "Weld with backing and all fillet welds".
Thanks & Regards,
(Karthik)
Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Fax : +66 38 897 034
Hand Phone: 0066 892512282
From: John Henning <jhenning@deltak.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, October 3, 2012 3:07 AM
Subject: [MW:15449] RE: 15448] Welding Procedure - Monel to Monel
No
John A. Henning
Welding & Materials
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of prashant pansare
Sent: Tuesday, October 02, 2012 8:09 AM
To: mat wel
Subject: [MW:15448] Welding Procedure - Monel to Monel
Sent: Tuesday, October 02, 2012 8:09 AM
To: mat wel
Subject: [MW:15448] Welding Procedure - Monel to Monel
Dear All,
I am qualifying Welding Procedure - Monel to Monel butt weld with CS backing.
On basis of the same can I qualify Welding Procedure for Monel to CS in fillet position?
Regds,
Prashant Pansare
(IRS - Mumbai)
(IRS - Mumbai)
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment