Re: Re: [MW:13582] Ultrasonic Testing & Intergranular Corrosion Testing; G28 Method A for CRO Welding on Carbon Steel with Inconel 625

Hi,

Generally not required, but if Client insist to do so and pay for extra cost then go for it.

But performing these tests may be useful in future if ever encounter a client requesting the
same, in that case you might have to carry out new qualification, i have seen major
manufacturers doing these tests just to make sure that they do not re-qualify if ever client
request UT,Intergranular corrosion test..

Regards
Manpreet Singh


On Mon, 30 Jan 2012 14:47:24 +0530 wrote
>No requirement of UT & Intergranular corrosion tests.

Thanks
Regards
E.Jegan
Hp-65-96163449

>



From: Ghafor Mohamad
>To: materials-welding@googlegroups.com
>Sent: Saturday, 28 January 2012 2:28 PM
>Subject: [MW:13576] Ultrasonic Testing & Intergranular Corrosion Testing; G28 Method A for CRO
Welding on Carbon Steel with Inconel 625
>
>

Dear Experts
>
>I am qualified a PQR for CRO Welding using Inconel 625 on Carbon Steel plate. As per ASME IX,
mandatory test is:
>

Dye Penetration Test
>
Transverse Side Bend Test
>
Chemical Analysis
Hardness (location may refer to ISO 15056 Fig 6 for NACE req.)
Macro Etch photo
What I am confusing is that Intergranular Corrosion (G28 Method A) and Ultrasonic Test is
applicable to conduct or not?
Thanks
BR; Abdul Ghafor Mohamad

>--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
>

>
>



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
>

Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...