Tuesday, January 31, 2012

Re: [MW:13584] Pipe damaged during fabrication

You need to make commonly weld build up procedure ad submit to Client for Approval ...Once Client accept the the procedure ...you may proceed for further repair ,It is very important thing is you need to make sure that after the repair base metal completely free from defects by using NDT Methods . 

Regards

Suresh

On Mon, Jan 30, 2012 at 7:52 PM, jesti fer <jesti_fer@yahoo.com> wrote:
Dear Experts,
I have problem in our site that, we found some fabricated pipes ( as per B31.3) the parent material thickness reduced by grinding (or due to any handling mark) more than 12.5% is not acceptable,
is there any possibility to build up (Buttering) the base metals. Where can I will get the reference
 
jestifer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 974 -  5 5 4 3 1 7 8 8  /  7 7 1 3 4 5 9 0 . ( Qatar )

 
                  91 - 92 92 905 905 ( India )

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...