Re: [MW:13577] Ultrasonic Testing & Intergranular Corrosion Testing; G28 Method A for CRO Welding on Carbon Steel with Inconel 625

No requirement of UT & Intergranular corrosion tests.
 
Thanks
Regards
E.Jegan
Hp-65-96163449

From: Ghafor Mohamad <ghaformohamad@gmail.com>
To: materials-welding@googlegroups.com
Sent: Saturday, 28 January 2012 2:28 PM
Subject: [MW:13576] Ultrasonic Testing & Intergranular Corrosion Testing; G28 Method A for CRO Welding on Carbon Steel with Inconel 625

Dear Experts

I am qualified a PQR for CRO Welding using Inconel 625 on Carbon Steel plate. As per ASME IX, mandatory test is:
  1. Dye Penetration Test
  2. Transverse Side Bend Test
  3. Chemical Analysis
  4. Hardness (location may refer to ISO 15056 Fig 6 for NACE req.)
  5. Macro Etch photo
What I am confusing is that Intergranular Corrosion (G28 Method A) and Ultrasonic Test is applicable to conduct or not? 
Thanks
BR; Abdul Ghafor Mohamad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...