Friday, January 20, 2012

Re: [MW:13525] Regarding welding consumable for Material hastelloy C276


Use ERNiCrMo4/ENiCrMo4 for welding between C276 TO C276 or to any austenitic SS. 

Regards,

Zakir Ali.


From: james gerald <gerry_tup@yahoo.com>
Sent: Fri, 20 Jan 2012 10:08:48
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Subject: Re: [MW:13501] Regarding welding consumable for Material hastelloy C276
Please use ER/E NiCrMo4 welding consumables for  GTAW & SMAW processes for welding Hastealloy

and

ER/E NiCrMo3 welding consumables for Hastealloy to SS316L
 
Thanks & Regards

J.Gerald Jayakumar
0091-9344954677

From: Vivek Pandey <vivek.pande06@gmail.com>
To: materials-welding@googlegroups.com
Cc: pgoswami@sympatico.ca; karthik6684@yahoo.com
Sent: Wednesday, January 18, 2012 11:02 AM
Subject: [MW:13499] Regarding welding consumable for Material hastelloy C276

Dear All

With reference to above subject,kindly suggest me which Consumable is
suitable for welding of hastelloy C276 material( UNS NO: N10276 ).
actually I want to do qualify in two different procedure.
preocedure are as follows

Material: UNS NO:N10276+UNS NO: N10276                PROCESS GTAW+ SMAW

Material: UNS NO:N10276 +SA182 GR 316L    PROCESS GTAW+ SMAW


KINDLY CONFORM TO ME AS SOON AS POSSIBLE


Regards
vivek pndey

--
To post to this group, send email to materials-welding@googlegroups.com');" >materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com');" >unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...