RE: [MW:13522] P1+P4 Fiiler

 

If sub zero application is not there you can use simple E7018 also, Heat treatment could be required subject to code requirement and hardness observed after welding

 

 

regards

Ravinder Sharma

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of shahid riaz
Sent: Thursday, January 19, 2012 11:30 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:13519] P1+P4 Fiiler

 

Dear friends,

ER70-S2 is best to weld good quality of root pass & its better to use E7018-A1 for SMAW process.

 

Shahid

   

On Mon, Jul 11, 2011 at 11:33 AM, Naresh Kumar <snareshkumar30@yahoo.com> wrote:

Dear friends,

 

I have a doubt about SA106 B+SA335 P11 disimilar welding;Which electrode is best?? whether ER70S2 OR ER80S-B2;

 

Regards,

S.Naresh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...