Hi,
ER80SB2 is the suitable one.
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Fax : +66 38 897 034
Hand Phone: 0066 892512282


From: shahid riaz <shahidriazkhan@gmail.com>
To: materials-welding@googlegroups.com
Sent: Friday, January 20, 2012 1:00 AM
Subject: Re: [MW:13519] P1+P4 Fiiler

Dear friends,
ER70-S2 is best to weld good quality of root pass & its better to use E7018-A1 for SMAW process.

Shahid
   

On Mon, Jul 11, 2011 at 11:33 AM, Naresh Kumar <snareshkumar30@yahoo.com> wrote:
Dear friends,

I have a doubt about SA106 B+SA335 P11 disimilar welding;Which electrode is best?? whether ER70S2 OR ER80S-B2;

Regards,
S.Naresh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...