Re: [MW:13515] Diff b/n Normalising and Normalised Rolling Reg.,

Dear KCR,
Normalised Rolling - Rolling of the ingot to plate form ( or any finished product) at the Normailising temperature say around 900 Deg.C.
Normallising - Heating up the finshed product after production to normalising temperature and cooling in still air.
Thanks and Best Regards,
K.Rajagopal

On Thu, Jan 19, 2012 at 4:20 PM, kcrtechnical <kcrtechnical@gmail.com> wrote:
Dear Freinds,
 
Can any one tell me the difference between Normalising and Normalised rolling
 
Best regards
K C R

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...