Thursday, January 19, 2012

Re: [MW:13508] RE: 13498] compatible forging material for SA 517 grade E plate

Dear Mr. Hemant,

Pl check SA 592 Gr. E. which is compatible with SA 517 Gr. E.

With Best Regards,

Jignesh R Rana
Manager - Materials Technology, QA/QC & Standards

Linde Engineering India Pvt. Ltd.
'Linde House'
Opp: VUDA Office, VIP Road, Karelibaug,Vadodara - 390018, India.
Tel.: +91 265 3056789, Fax: +91 265 2335213 , Mobile: +91 90999 86019
jignesh.rana@linde-le.com, www.linde-india.com

This e-mail is confidential. If you are not the intended recipient, please notify us immediately. You should not disclose its contents to any other person nor use it for any purposes.




"pgoswami" ---19-01-2012 09:09:54---Hi Hemant,

From: "pgoswami" <pgoswami@quickclic.net>
To: <materials-welding@googlegroups.com>
Cc: <c2hemant@gmail.com>
Date: 19-01-2012 09:09
Subject: [MW:13506] RE: 13498] compatible forging material for SA 517 grade E plate
Sent by: materials-welding@googlegroups.com





Hi Hemant,

It's difficult to find the exact compatible forging grade to SA 517 steel. You may have to select grade which may be close, though not exactly similar in chemical composition. What're the grades you've in mind?
Why did you select SA 517 Gr E for a high temperature component like steam drum. Is there any compelling reason for the same and what the design conditions are?

This steel is not exactly welding friendly and there could be all sorts of issues at higher thickness.

See the attached catalogue, for your reference. Note ASTM A 514 and SA-517 steel are of back to back composition.


Thanks.



Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario, Canada.
Email-pgoswami@sympatico.ca,
pgoswami@quickclic.net

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of hemant chintamani
Sent:
Tuesday, January 17, 2012 1:07 PM
To:
materials-welding@googlegroups.com
Subject:
[MW:13498] compatible forging material for SA 527 grade E plate

To the experts,

I am designing steam drum using SA 517 grade E plate material in ASME Sec, VIII, Div. II. For this please suggest me a compatible forging material for designing of nozzles.

--
Thanks & regards,

Hemant B. Chintamani

Sr. Design Engineer,
ISGEC Heavy Ind. Ltd.,
India.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
_
This mail item contained either a password protected, encrypted or unscannable attachment and could not be checked for viruses. The attachment is removed based on Linde corporate policy. If you require this file for business reasons please contact your local helpdesk with the request to release it to you.


The file(s) was:
ARCELORMITTAL A514 AND T-1.pdf

Removed by:gweua3adm.linde.grp

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...