Hi

 

// I have problem in our site that, we found some fabricated pipes ( as per B31.3) the parent material thickness reduced by grinding (or due to any handling mark) more than 12.5% is not acceptable,//

 

I would like to clarify that, the 12.5% reduction in thk, mentioned by you is taken from material specification. Not from ASME B31.3. B31.3 specifies only the minimum thickness. See 304. So, it is Designers decision to say whether this piping can withstand the intended service or not.

 

See 328.4.2 (b)(4) and 328.4.3(c) for base metal repairs pertaining to alignment. But, for base material repairs on other areas, B31.3 neither specify nor prohibit.

 

In these situations, If the thickness is found to be less than the minimum required thickness, and confirmed by Designer/Owner,

you may do the repair as per material specification and carryout the necessary inspection.

 

Note that any repairs on the parent material requires owners/purchasers prior approval and done with the qualified procedure/welders.

 

BR

M.Vijayan

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of jesti fer
Sent: Monday, January 30, 2012 5:23 PM
To: materials-welding@googlegroups.com
Subject: [MW:13583] Pipe damaged during fabrication

 

Dear Experts,

I have problem in our site that, we found some fabricated pipes ( as per B31.3) the parent material thickness reduced by grinding (or due to any handling mark) more than 12.5% is not acceptable,

is there any possibility to build up (Buttering) the base metals. Where can I will get the reference

 

jestifer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



This communication and any files transmitted with it are confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient or the person responsible for delivering it to the intended recipient(s), please note that any form of distribution, copying or use of this communication or information contained in it is strictly prohibited and may be unlawful. If you have received this communication in error please return it to the sender, and delete the material from any computer. We reserve the right to monitor email communications through normal internal and external networks. We believe but not warrant that the email and the attachments are virus free. The statement and opinions expressed in this communication are those of the writer and do not necessarily represent those of Madina Group, whose registered office address is

P.O. Box 20459, Doha, Qatar.
Tel. +974 44600818
Fax. +974 44603143

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...