DEAR,

 

Is GTAW is required?

We used SMAW or GMAW for the root and remaining for with FCAW or GMAW which is more economical and good work progress.

 

Thanks and Regards................?

 

Lakshman Kumar.B|Manager |Lanco Infratech Limited

Plot No 1255 | Sanjeevani chowk | Mahanadi vihar | Cuttack 753004

Phone : + 91 671 2445033 | Mobile : +91 9937286851 |www.lancogroup.com

Go Green|The future will thank you

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Mohamed Elsayed ( BTG)
Sent: Tuesday, January 24, 2012 9:42 AM
To: materials-welding@googlegroups.com
Subject: [MW:13556] Welding API 5L X70 By ER 80S-Ni1 + FOX EV 60

 

Dear,

 

We have material  API 5L X70 , 30” O.D ; Thk. 13.33mm , we are planning to do PQR using ER 80S-Ni1(mod) 2.4mm for GTAW and E8018-C3H4R – Bohler welding consumable. Is it correct?

 

Please advice.

 

 

Thanks

Mohamed

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...