[MW:13553] PWHT requirements -ASME B31.3

Dear all

My question is that  if a 15 mm build is to be carried out on a 25 mm thick flange face, would I require to do a post weld heat treatment? What would be the governing thickness in this case?
Section 3331.1.3 states that governing thickness shall be that of thicker component measured at the joint except in case of branch and fillet.
So does that implies weld joint? i.e. 15 mm in this case?

Any supporting document (eg ASME clarifications) would be much appreciated.

Thanks in advance.

Best regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...