[MW:13546] Re: Valve Back Seat Test

Dear Gobi

Backseat will be done for gate and globe valve...That is nothing but
the handle will be opened fully and this test main purpose of stem
seat.
The test pressure is 1.1 times of MOP.

Regards

Santhosh
On Jan 20, 11:01 pm, Gopi Perumal <parinitaa2...@gmail.com> wrote:
> Dear all,
>
> Anybody can explain what is mean by Backseat test in Valve Testing? (API 598)
>
> Thanks,
> P Gopi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...