Dear Gopi,

Valve back seat tests are done in Gate and globe valves

It's done by opening the valve to the fullest and loosening the packing
gland and pressurizing the shell.

It's done at 1.1 times the maximum allowable pressure at 38 °C (100 °F)

Cheers
MM


-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Gopi Perumal
Sent: Saturday, January 21, 2012 8:01 AM
To: materials-welding@googlegroups.com
Subject: [MW:13531] Valve Back Seat Test

Dear all,

Anybody can explain what is mean by Backseat test in Valve Testing? (API
598)

Thanks,
P Gopi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...