Saturday, January 21, 2012

[MW:13536] REGARDING PWHT of STORAGE TANK CLEAN OUT DOOR.

Dear All,

I intended to use the following  WPS  for  storage tank clean out door welding :

Test coupon thickness  -   40 mm.
Material                       -   SA 516 Gr 70
Welding process          -   SMAW.
Electrode                    -    E 7018-1
PWHT  Temperature     -   620 - 650 degree centigrade.
Soaking time               -   180 minutes.
Rate of heating            -   130 Degree centigrade.
Rate of heating            -   130 Degree centigrade.

Storage tank detail:
Shell thickness              - 18 mm
Annular plate thickness  -  20 mm
Clean out door neck       -  18 mm
Clean out door flange      -  20 mm
Material                         -  SA 516 Gr 70
Welding process            -   SMAW
Electrode                       -   E 7018 -1
Stress relieving temp      -   620 - 650 degree centigrade.  
Soaking time                 -   60 minutes.
Rate of heating              -   150 - 200 Degree centigrade.
Rate of heating              -   150 - 200 Degree centigrade

My doubt is whether the soaking time in the PQR is acceptable or I have to qualify another WPS.

Thanks in advance.
Manoj

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...