[MW:13535] wELDING CONSUMABLES for BSEN 10025 - 355 JO and HT 12.9.9 grade bolt

Dear friends ,

Greetings to all.

I have to weld 355 JO of 50mm thickness plate with high tension round bar of 32
diameter of 12.9 grade.

Please note that already I have one PQR for API grade 65 which was qualified with
E8018G electrodes. Whether it is suitable to weld or new PQR has to be established?
Which electrode will be suitable to weld 355JO of 50mm thickness with 12.9grade HT
round bar of 32mm thickness?

Hi friends your reply is highly appreciable .



Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951
Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...