[MW:13499] Regarding welding consumable for Material hastelloy C276

Dear All

With reference to above subject,kindly suggest me which Consumable is
suitable for welding of hastelloy C276 material( UNS NO: N10276 ).
actually I want to do qualify in two different procedure.
preocedure are as follows

Material: UNS NO:N10276+UNS NO: N10276 PROCESS GTAW+ SMAW

Material: UNS NO:N10276 +SA182 GR 316L PROCESS GTAW+ SMAW


KINDLY CONFORM TO ME AS SOON AS POSSIBLE


Regards
vivek pndey

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...