Re: [MW:12166] Effect of PWHT - - SS 410 Overlay on SA 516 (Carbon steel)

Dear Mitul:

  1. Is it  (410s) or (410)...?
  2. Did you deposit any buffer layer or directly deposited 410 in A516...?

    please send your WPS or describe it in more details... because it makes a big difference...

Regards
Ramin  Kondori
   QC/Welding Engineer 
         IWE AT 0070
   



On Tue, Aug 9, 2011 at 11:24 AM, mitul patel <mitulmrpatel@gmail.com> wrote:
Dear All

In one of the NACE requirement  equipment, some of the parts of Carbon steel SA 516(20 mm Thk.) is overlaid by SS 410 (3 mm). PWHT has been asked by customer after overlay.
Can anybody tell the effect of PWHT on SS 410 overlay?
What will be the the safe range of temperature of PWHT?

Regards,
Mitul Patel




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...