Re: [MW:12162] ASME Section VIII Div. 1 : Query about stiffener ring on insert plate

Dear Joshi,
First you have to Radiograph the area at which the stiffener ring passes. On satisfactory review, you can weld the Stiffener ring crossing the insert plate.
Thanks and Best Regards,
K.Rajagopal

On Tue, Aug 9, 2011 at 7:56 AM, Joshi <joshi@knm-group.com> wrote:

Dear All,

 

Request your kind expert advice on below query.

 

Vessel have Nozzle with Insert plate. External pressure stiffener ring is passing over Insert plate. Is this allowed as per code? Can we notch the stiffener ring to suit the insert plate shape outside vessel? Shift of Stiffener ring is not possible to no space available..

 

Request your prompt positive advise.

 

Thanks and best regards

 

Joshi

 




***DISCLAIMER NOTICE: ***

"The information contained in this email and/or any attachment hereto is strictly confidential and privileged. If you are not the intended recipient, and/or have received this email in error, you must not copy, disseminate or disclose the contents of this message and/or any attachment to any other person. Please notify the sender and delete this message and any attachment from your system. KNM accepts no liability in respect of prohibited and unauthorised use by an unintended addressee or recipient. Any personal views or opinions expressed by the sender shall be understood as neither given nor endorsed by KNM or any of the companies within the Group. Although this email and/or any attachment is believed to be free of any virus or other defect which may affect any computer system into which it is received and opened, it is the responsibility of the recipient to ensure that it is virus-free and KNM accepts no responsibility for any loss or damage arising in any way from the use thereof."




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...