Re: [MW:12159] Requirement of MPT or LPT on bevel ends of butt weld fitting.

 
It depends on case to case and requirement of specification.
No standard has asked for it, unless otherwise specified by Clients.
Moin-Pune
On 7 August 2011 18:02, sreeraj panicker <sreerajmannar@gmail.com> wrote:
Dear's,
         Is it any where mentioned in STANDARDS that all bevel ends of carbon steel butt weld fittings, NDT should be carried out such as LPT or MPT by the manufacturer.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...