Re: [MW:12140] welding position limitations for SMAW & GTAW

As far as process is concerned ( GTAW&SMAW), suitable for all position but in SMAW based on Electrode Classicification, position is restricted
Pandithan

On Wed, Aug 3, 2011 at 11:55 PM, abdul khan <abdul_khan2010@yahoo.co.in> wrote:
Dear Experts ,
 
can any one say The welding postioin  limitations for SMAW & GTAW .
 
It will be appriciated  if you mention  reff Standard.
 
Waiting for Reply from weldiing Experts .
 
Regards.
ABDUL JABBAR KHAN

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...