Re: [MW:12136] RE: 12112] Regarding PT & MPI test on overhead position

Hi,
Overhead position you can apply PT conveniently,In MT during apply magnetic particle you face some problem ie fall over inspector. In PT you  use Solvent removable method you can eliminate .
Thanks
Regards
S.Eswaran
ASNT NDT Level III (PT,UT,RT&MT)
0065-83495961


From: Pieper QSI <pieper-qsi@kpnmail.nl>
To: materials-welding@googlegroups.com
Sent: Friday, 5 August 2011 3:48 PM
Subject: [MW:12113] RE: 12112] Regarding PT & MPI test on overhead position

Dear Sir,

You can apply both technologies in the overhead position. There are no
restrictions for these technologies regarding execution position. 

Met vriendelijke groeten / Best Regards

Herman Pieper

Pieper Quality Support & Inspection
Phone: +31 (0)521 380083
Fax:    +31 (0)84 7539225
Cell:    +31 (0)6 51691215
www.pieper-qsi.nl

-----Oorspronkelijk bericht-----
Van: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] Namens khatri ankit
Verzonden: vrijdag 5 augustus 2011 9:25
Aan: Materials & Welding
Onderwerp: [MW:12112] Regarding PT & MPI test on overhead position

Dear Experts,

I just want to know that in overhead position which NDT method is
suitable either DPT or MPI

Kindly mention the significance for the same.

y it's used ? and y it;s not used?

Regards,

Ankit Khatri

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...