Re: [MW:12129] BS970 304 S15

Austenitic SS low carbon grade

On Sat, Aug 6, 2011 at 4:08 PM, QC TMAK <qc.tmak@technomakfzc.ae> wrote:
> Gents,
>
>
>
> Anybody aware about the below material grade.
>
>
>
>  BS970 304 S15

>
> Thanks & Regards,
>
>
>
> Sandeep.K.P
>

--