Re: [MW:12103] PWHT near to Tempering temperature for SA350 LF2 CL 1 Flanges

Dear,

Some of the reputed specification like Foster wheeler recommends the tempering temprature atleast 10 greater than PWHT temprature. In your case i there should not be any technical problem if you accept the same.As far as contract point of view you should be ready with a proof that it is satisfaying the requirement of job(Mechanical properties).

Regards,
VJ

SA 350 LF2 is prob. a ASME P1 material which calls min PWHT temprature


On Wed, Aug 3, 2011 at 2:57 PM, asad azmi <azmiasadayub@gmail.com> wrote:
Dear All,
 
Greetings.
 
As per  UOP # 3-12-5 para 4.1.i.
The tempering temperature for tempered material shall be at least 50 ºF (28 ºC)
greater than the maximum intermediate or postweld heat treatment temperature
.
 
Consttuction code - ASME SEC VIII DIV 1, Flanges are SS 316L overlaid in ID and Gasket face. 
 
During review of MTC for SA 350 LF2 CL 1, Flanges Tempering Temperature observed  greater by  10  deg celcius from PWHT Temperature.
 
Details are as bleow --
 
Flanges are supplied in Quenched and Tempered condition. Tempering temperature is 630 deg celcius.
 
PWHT temperature for the vessel is  620 deg celcius( minimum).
 
Please suggest whtether this can be accepted.
 
Thanks & Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...