Wednesday, August 3, 2011

Re: [MW:12079] SMAW - Welding Electrode Holder

Hi Sir,

Please check this website www.zrid.us.

 ZRID uses a wireless trigger and isolation device system to switch OFF the secondary circuit of the welder to provide 0 Volts in the welding cable during non arcing operation,dramatically reducing the window of opportunity for exposure to electrical shock Hazard.

If any details,please conduct SINGAPORE WELDING SOCIETY.

This product dealer in Malaysia.

Regards,
Senthil.M

On Thu, Jul 28, 2011 at 11:28 AM, Ash_Ish Soni <ashishsoni18@gmail.com> wrote:
Dear Member,

I have come across to know that our contractor is using Welding Electrode Holder as per the attached photo. Contractor is big enough to force without standard, so, I am searching for any International Standard which helps to force them to replace this kind of Welding Electrode Holder with the Standard one, which all of you know.

I have come to know one standard - IEC - 60974 - 11, but that is only for Safety point of view, which is not enough.

Request for the help.

Thanks & Regards,

Ashish Soni.
Essar.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...