Re: [MW:12075] 0.2% offset method

Dear Prashantpan:

In some materials, the stress at which the material changes from elastic to plastic behavior is not easily detected.

In this case, the offset yield strength is determined. A line is constructed parallel to the initial portion of the stress-strain curve but offset by 0.002 in/in (0.2%) from the origin.

The 0.2% offset yield strength is the stress at which the constructed line intersects the stress-strain curve as shown:
0.2% offset method.png


Regards
Ramin  Kondori
   QC/Welding Engineer 
         IWE AT 0070
   



On Wed, Aug 3, 2011 at 8:43 AM, Ramin Kondori <raminkondori@gmail.com> wrote:
Dear Prashantpan:

In some materials, the stress at which the material changes from elastic to plastic behavior is not easily detected.

In this case, the offset yield strength is determined. A line is constructed parallel to the initial portion of the stress-strain curve but offset by 0.002 in/in (0.2%) from the origin.

The 0.2% offset yield strength is the stress at which the constructed line intersects the stress-strain curve as shown:


Regards
Ramin  Kondori
   QC/Welding Engineer 
         IWE AT 0070
   



On Tue, Aug 2, 2011 at 6:29 PM, prashant pansare <prashantpan_99@yahoo.co.in> wrote:
Dear All,
In some of the materials we need to go for 0.2% offset method for Y.S. Why?
& 0.2% of which value is to be calculated?
Thanx & Regds,
PSP

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...