Tuesday, August 2, 2011

Re: [MW:12056] Single bevel PQR can we use as backweld

Dear Mr. Bharat

Yes you can use same PQR for back weld.  For Your More Detail You Red ASME Sec IX QW-306 for combination of welding processes & as Per Table QW-253 ( QW-402 all points are nonessential.) 

Thanks & Regards,

Vijay Malusare.
(Sr. QA/QC Engineer.)

Mob No. : 09904213726

On Mon, Aug 1, 2011 at 2:54 PM, arvinda shan <arvindashan@gmail.com> wrote:

Dear friend,
 
You have already PQR for both root and cap. Then u can procced with that PQR for making WPS.
 
Arvinda.

On Sun, Jul 31, 2011 at 3:24 PM, BHARAT GOLE <bharatgole@hotmail.com> wrote:
 I have PQR with for single bevel with E6010 root & E7018 for fill & Cap as per ASME IX
Can I prepare WPS with back weld with help of same PQR.....only using E7018 ?
Expert your comments pl with ref to ASME Clause
Regards
Bharat


 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




 
 
 
 
Please Don't Print This e-mail Unless You Really Need to. Save a Tree If Possible.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...