Monday, August 1, 2011

Re: [MW:12048] change in welding Technique does it require Requalification ?

Dear Abdul ..
 
First you need to mentioned clearly that for what requalification needs? ,Welder perfomance or Procedure Qualification ?
 
Suresh

On Mon, Aug 1, 2011 at 6:11 PM, abdul khan <abdul_khan2010@yahoo.co.in> wrote:
Dear Experts,
 
 
If the welding technique is changed does it require Requalification ? as the QW-401.2  it states.
 
QW-401.2 Essential Variable (Performance).
A change in a welding condition which will affect the ability of a welder to deposit sound weld metal (suchas a change in welding process, deletion of backing, electrode, F-Number, technique, etc.).

 

were as the  QW-401.1 Essential Variable (Procedure). it states Welding technique as Non-Essential variable .

 

Which QW we have to follow  and why ?

 

comments plzzzzzzzzzzzzzzzz.

 

Regards

ABDUL JABBAR KHAN

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...