[MW:12128] API storage tank settlement tolerance.

Dear All,

I have one storage tank to erect at site as per API 650.  The size of the tank is 54 meter diameter and during water fill up test we have to measure settlement.  Can any body give me information about tank settlement tolerance and in which standard it is specified.

Thanks,
Regards.
Manoj

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com