> Hello Everybody.
>
> Good day to you all. It has been long time since my last blog.
>
> I would like to get responses from experienced members who have actual
> experience with tantalum to provide any recommended practices and any
> international code reference details with regard to the subject
> material system.
>
> Any alternative methods adopted, like cladding or alternative
> materials used like glassteel are also welcome. Tantaline experience
> is most welcome.
>
> Actual documents and propreitary information are not sought here. Only
> reference information available from public domain is sought.
>
> Issues concerning are availability, reliability, sizes, design (Stress
> issues), welding complexity, welding qualifications, fabrication
> feasability at field, for Tantalum and other alternative types
> proposed as indicated above.
>
> Thanks.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...