RE: [MW:11225] any one can explain how welding CRACKS looks on x-ray film of any welded pipes ETC. ----

Rgds

raj                                                                                                                                                                                     

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Chandrahas Rathod
Sent: Tuesday, May 31, 2011 09:45
To: materials-welding@googlegroups.com
Subject: Re: [MW:11220] any one can explain how welding CRACKS looks on x-ray film of any welded pipes ETC. ----

 

hi,
it will be straight under lower mag and same will be in zig-zag/tapered in both direction under high mag.
each zig-zag point connects to make a straight line(H .mag).
under low mag u can see zig-zag only if the residual/ service stress is high enough to reveal it and it will be not straight at normal mag.


On Sun, May 29, 2011 at 2:24 PM, sajidalam mohd. <engineer_makes_world@yahoo.co.in> wrote:

DEAR EXPERTS

                     GOOD DAY

CAN ANY ONE EXPLAIN HOWS CRACKS IN WELD ON X-RAY FILMS LOOKS?

 

IT LOOK LIKE ZIZ ZAG???

ITS LOOKS LIKE THIN/NARROW STRAIGHT LINE???

 

BECAUSE I AM  CONFUSED ABOUT INDICATION OF CRACKS OF WELDING ON X-RAY FILM?

 

 

WAITING FOR REPLY.

 

REGARDS

MOHAMMAD SAZID ALAM

INSPECTION ENGINEER

AICO-DAMMAM

MOBILE:-0534077860

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--

_____________________________________________________________________________________

 

C . R . RATHOD
PhD Student

SCHOOL OF MECHANICAL,MATERIALS & MECHATRONIC ENGINEERING

SMART BLDG 6,  ROOM NO: 107

UNIVERISTY OF WOLLONGONG - 2522

NEW SOUTH WALES 

AUSTRALIA

 

M   : +61434059865
P    : 04239 2356

 

______________________________________________________________________________________

 

Minds are like parachutes - they only function when open. - Thomas Dewar
_____________________________________________________________

If you do not understand my silence, you will not understand my words
_____________________________________________________________

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...