Limesh,

The welder can be renovated perfectly by the suggested method, see QW-320.

Regards

 

Di Prinzio, Juan Carlos

 

De: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] En nombre de jaya anil
Enviado el: lunes, 30 de mayo de 2011 7:32
Para: materials-welding@googlegroups.com
Asunto: Re: [MW:11208] Renewal of Welder Qualification

 

Dear Limesh,

 

Just see clause 452.3 in ASME Sec.IX, there are Diameter restrictions, you have qualified your welder in 1 1/2 " Pipe means he falls in 1"(25mm) to 2 7/8"(73mm) restriction, which says Welder can weld from 1" to unlimited, but now for his renewal you are supporting 8" pipe, So asthetically it is not possible, he may fall in over 2 7/8" ( ie 73mm to unlimited), So better to show RTs of 1 1/2" or less than 2 7/8" Pipe . So that he can regain his qualification subject to his contuity record.

On Sat, May 28, 2011 at 6:29 PM, limesh M <limesh78@gmail.com> wrote:

Dear All,

 

Welder Qualification Code: ASME BPV SEC IX

 

I have a qualified welder with following diameter range.

 

1.1/2'' and above

 

 

Now his qualification is going to expire and I would like to renew it by showing supporting radiography reports.

 

Is it possible to renew the above qualification by showing the radiography report of an 8" diameter pipe?

 

 

Regards,

 

Limesh 

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

__________ Información de ESET Smart Security, versión de la base de firmas de virus 6164 (20110530) __________

 

ESET Smart Security ha comprobado este mensaje.

 

http://www.eset.com



__________ Información de ESET Smart Security, versión de la base de firmas de virus 6164 (20110530) __________

ESET Smart Security ha comprobado este mensaje.

http://www.eset.com

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...