Re: [MW:11107] Use group III filler metal and flux classification for the welding of Group II base metal?

in ASTM there is no exact equivalent grade for S355j2. for this type of material specify it as a unassigned material.

On Thu, May 19, 2011 at 2:09 PM, mhaskar Aly <mhaskar.aly@gmail.com> wrote:
Dear All
 
Kindly spare your valuable time & note following & reply me, thanks in advance. 

 

 

Used base  metal grade :-

 

BSEN 10025  Grade – S355J2

Yield Strength ---- 355N/mmSq. Min

Tensile Strength---- 490 TO 630N/MMSq.

Elongation – 22% Min

 

 

 

Al Babtain following AWS D1.1 Code  for  welding and  preparing   WPS/ PQR in line  with selection of base  metal and  filler metal  combination for matching strength from table 3.1. in the above case since  the base  metal is  according to European norms and not covered in AWS D1.1  table 3.1 but it approximately  equivalent to ASTM  A 572 Gr. 50 which tensile strength is 450N/mmSq Min.  and Yield Strength 345 N/mmSq. Min. ---- Group II as per table 3.1

 

 

However, In  actual for  welding  of   said  material  grade S355J2 we used our  qualified  SAW procedure   which is prepared against  group III  Material ASTM  A 572 Gr. 60. with filler  wire and  flux classification is F8A4-EA3K-A4

 

Now my Query is  could  we use group III  filler metal and  flux classification for  the  welding of Group II base  metal?

 

If you have any equivalent grades table please forward me.

 

 BSEN ISO 10025- Grade S355J2 which grade is equivalent in ASTM material

 

 

Thanks with  best regards,

 

 

 

 

Mhaskar Aly
kuwait

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
THANKS & REGARDS
 
KALYAN VVV
WELDING ENGINEER
THYSSEN KRUPP INDUSTRIES (INDIA) LTD
HYDERABAD
Mob.NO- 09885273257

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...