Hi,
 
There will be some design flow rate for the fluid through the pipe. If we do butt welding in small pipes, it will obstruct the flow when the root penitration is more. That's why it is recommented to do socket welding.
 
Thanks & Regards
Muhammed Ibrahim PK



On 2 March 2011 20:51, jagadish.dodiya@gmail.com <jagadish.dodiya@gmail.com> wrote:
Why small bore piping is socket welded?
can i butt weld smallbore piping?
reson is bore geting ruduce OR less thichness?

regards,
Jagdish

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...