Re: [MW:10165] FCAW -4G -WPS & WPQ is possible or not ? Most urgent

Hi,
 
Make a pipe fitup in 6G position and try to weld it with FCAW. If the radiograpghy gives good result, you can proceed. Some brands/batches may not give good result.
 
Thanks & Regards
Muhammed Ibrahim PK



On 19 February 2011 17:01, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:
Dear All.

pl clear me on tat.
Can We Qualidy WPS & WPQ in FCAW Process in 4G position is possible or
not?
Code is AWS D1.1.
Is any practical problem in tat?
Its urgent/


Thanks & Regards

Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...