RE: [MW:10095] PWHT

Heating and cooling rates not specified in ASME B31.3 except which states uniformity of the temperature to be maintained while Heating and cooling.

 

The above is from ASME Sec.VIII Div.I which can be used.

 

J.Gerald

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of k.ilangkumaran ilangkumaran
Sent: Tuesday, March 01, 2011 7:47 PM
To: materials-welding@googlegroups.com
Subject: [MW:10079] PWHT

 

Dear experts,

 

                  As per the ASME B 31.3 table 331.1.1 the temperature range is 704-746 deg C. How do we find out the rate of raising and cooling temperature?

 

Regards

Ilan

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Confidentiality Notice

This communication and the information it contains:-
(a) Is intended for the person(s) or organisation(s) named above and for no other person(s) or organisation(s).
(b) May be confidential, legally privileged and protected in law. Unauthorised use, copying or disclosure of any of it may be unlawful. If you have received this communication in error, please contact us immediately by email at Postmaster@fwuk.fwc.com.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...