Mr.Abdul, Stainless steels are selcted for their corrosion resistance, and that is due to the presence of Cr2O3 passive film layer on the surface, When welded without purging gas the chromium around the weld joint will react with the atmospheric oxygen and then form heavy scales ofcourse it depends on the thickness of the process pipe wall thickness and the heat input that you apply. some people may recommend to do IGC testing on the test samples done without purging, and for your surprise the results can also be acceptable, but it is not what we wanted. If you concern is cost factor of purging the line with Argon, I would recommed to use nitrogen as purging / backing gas which is a cost effective way in these kind of situation. In short any process pipe wall having thickness less than 6.3mm, there has to be backing gas when welding. Regards, Praveen Muscat --- On Fri, 12/24/10, abdul naveed <naveedhhi@gmail.com> wrote:
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments