Sir

We use ArCO2 but our operators say eye irritation & more porosity occur in
jobs we use gas flow in pipe line not in cylinders anybody can clarify.

Thanks & regards
V.S.Kumar


-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Srinivas Engr
Sent: Wednesday, December 29, 2010 8:01 PM
To: Materials & Welding
Subject: [MW:8992] Re: difference between MIG & MAG Welding

Hi

MIG - Metal inert Gas Welding By with Inert gases Like Argon & Helium
MAG - Metal Active Gas Welding by with Active Gases like CO2 / with
oxygen.

Both above are called GMAW. MAG are mostly usable in construction with
CO2
I hope its clear...


Regards
Srinivas

On Dec 29, 5:26 pm, ASIM MUNIR <asimmunir....@gmail.com> wrote:
> Dear all
> please guide about MIG and MAG welding and difference also.
> thankx in advance.
>
> --
> Regards,
> MUHAMMAD ASIM MUNIR
> QA/QC INSPECTOR
> MOODY INT.
> CELL #+923007815592
>            +971566230102
>
> "QUALITY IS MORE IMPORTANT THAN QUANTITY"

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...