Dear Suresh,
 
Your question is not clear??? please be specific.
" Impact test missing for the material which you are going to weld or the material which is used for PQR " 
NACE MR 0175 is only sour service requirement, if IMPACT TEST is client requirement then SAMPLE to be drawn from each HEAT ( for the material which is going to be used for production ). 

On Thu, Dec 23, 2010 at 10:55 PM, suresh kochayatu <sureshkochayatu@gmail.com> wrote:


-- Dear gents,
 
MERRY XMASS & HAPPY NEW YEAR  to all of you .
 
 I have a PQR, 316 L for sour service with impact test, at -196 C. It is a client requirement. But the material test certificates doesnt shows any impact test results.  it shows MEETS THE MRO 175 requirements.  This MTC is acceptable with out impact test? ,  Shall I do the impact test on the above material?  and if it meets the client requirements  shall we use the same material for all the production? seeks your valuable advise and opinion above matter.
Suresh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards,
Tulasi Ram

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...