Procedure qualification as per ASME sec ix,

I have 2 PQR:-
                        *PQR 1-   GTaw-6mm thick 
                        *PQR 2-   Smaw- 15 mm thick

What would be the thickness renge for base and weld metal?

for combined WPS,  base metal thickness range shall be 1.5mm to 30mm, am i correct?