Re: [MW:8951] Hydrostatic Test


Dear Larry , usually the holding time for buried Piping should be 2 hours for the strength test and 24 hours for tightness test , while for above ground piping the holding time should be 30 minutes to two hours ( Depends on project Inspection ) providing that ALL welds should be accessible for visual inspection to any leak.

Regards,

Sohaib   


From: Larry <quality@unieng.com.au>
To: materials-welding@googlegroups.com
Sent: Wed, December 8, 2010 4:18:47 PM
Subject: [MW:8611] Hydrostatic Test

Hi There,

 

Is there any table on holding time on hydrostatic test as per ASME B31.3 NFS, or any table in ASME code that would refer to it?

 

Thanks in advance.

 

Larry Zarate

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...