Hi Shankar,
Burn-through (too much penetration) is caused by having too much heat input in the weld zone. Please check the current, over current may be one reason for burnthrough.It happen when the speed is very slow so you can increase the travel speed. Burn- through  can  also  result  from  having  an  excessive amount of root opening.
 
regards,
 
 
Arun S Das
 



From: shankark <shankark.qc@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Thu, 30 December, 2010 9:00:24 PM
Subject: [MW:9023] reason for burnthrough defect

we got BT defect in smaw process welding using E6010 for root, and
E7018 for hotpass, capping. what could be the reason for this defect
and how we can avoid it.

thanks,
shankar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...