Wednesday, December 29, 2010

Re: [MW:8981] Combination of PQR for WPS

Dear Raghuram,

i had an idea about 5-12mm w/o impact considering QW-200.4(b), but can you please throw some focus on (6-12mm)

I am sure, i am missing something, Can you please calrify?


Regards
Manpreet Singh





On Wed, 29 Dec 2010 12:57:26 , "Bathula Raghuram (Mumbai - PIPING)" <R.Bathula@ticb.com> wrote

5-12mm w/o impact, else 6-12mm

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of manpreet
Sent: Wednesday, December 29, 2010 12:03 PM
To: materials-welding
Subject: [MW:8974] Combination of PQR for WPS

 

Dear All,

Procedure qualification as per ASME sec ix,

I have 2 PQR:-
                        *PQR 1-   GTaw-6mm thick 
                        *PQR 2-   Smaw- 15 mm thick

What would be the thickness renge for base and weld metal?

for combined WPS,  base metal thickness range shall be 1.5mm to 30mm, am i correct?

Regards
Manpreet Singh


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...